1111 Holly Green Stoneware Glaze 1111P A very dark green, breaking to pale green where it thins. Recommended Cone 4-6
1113 Milk & Honey Stoneware Glaze 1113P A soft cream banded with peach and rust. Recommended Cone 4-6
1114 Gold Rain Stoneware Glaze 1114P A dark blue-black densely speckled with rust gold. Recommended Cone 4-6
1115 Moonscape Stoneware Glaze 1115P A mid blue broken into paler and darker bands. Recommended Cone 4-6
1117 Texture Chocolate Stoneware Glaze 1117P A dark purple-brown, breaking pale lilac. Recommended Cone 4-6
1122 Satin Mottle Stoneware Glaze 1122P A pale cream mottled with soft yellow-green. Recommended Cone 4-6