Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Spectrum  |  1121P

1121 Satin White Stoneware Glaze

A soft satin white, faintly warm.

$20

Suggested retail price. In-store prices and availability may vary by location.

This is one of Spectrum's 1100 series stoneware glazes. It fires to an opaque satin, so the clay body will not show through. Brush on three coats for full colour and fire to cone 5, which is where it will match the jar. It will fire anywhere from cone 4 to cone 6, 1190 to 1230°C, but expect the colour to shift a little at either end. Lead-free and AP non-toxic. Conforms to ASTM D-4236.

  • Cone 4 to 6, cone 5 recommended
  • A soft satin white, faintly warm
  • Opaque satin
  • Three brush coats
  • Lead-free and AP non-toxic
  • Conforms to ASTM D-4236