1170 Texture Mulberry Stoneware Glaze 1170P A coral red with pink banding and dark speckle. Recommended Cone 4-6
1173 Running Hot Chowder Stoneware Glaze 1173P A pale yellow banded with rust orange. Recommended Cone 4-6
1181 Texture Cloudburst Stoneware Glaze 1181P A pale yellow-green flecked with rust and blue. Recommended Cone 4-6
1183 Texture Dark Cloud Stoneware Glaze 1183P A mottled grey green with a dark teal band. Recommended Cone 4-6
1187 Clear Crackle Stoneware Glaze 1187P A clear glaze that fires to a fine crazed web. Recommended Cone 4-6
1193 Fire Engine Red Stoneware Glaze 1193P A bright red with a faint orange lean. Recommended Cone 4-6