Spectrum  |  1173P

1173 Running Hot Chowder Stoneware Glaze

A pale yellow banded with rust orange.

$24

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 1100 series is a cone 4/6 stoneware glaze, and this colour is reactive. It is made to move and change in the firing instead of laying down one flat colour, so the result depends on the temperature, how thickly it is applied and the clay underneath, and the same jar can look quite different on a different body. It is the most fluid colour in the line and will run on a vertical surface. Three brush coats give the full colour. A reduction firing gives a different result from an electric kiln. Lead-free. Spectrum does not rate it non-toxic in the liquid state.

  • Cone 4 to 6, cone 5 recommended
  • A pale yellow banded with rust orange
  • Reactive, varies with temperature, thickness and clay body
  • Three brush coats
  • More fluid than most, can run on vertical work
  • Lead-free
  • Not rated non-toxic in the liquid state