138 Clear Crackle Glaze 138P A clear gloss that crackles as it cools, showing the pattern once ink or dye is rubbed into the cracks. Recommended Cone 06-04
1424 Cactus Ash Glaze 1424P A translucent yellow-green ash that runs in streaks. Over 1145 it breaks to orange and rust with blue at the edges. Recommended Cone 4-6
1426 Blueberry Ash Glaze 1426P A translucent blue ash that runs in dark streaks. Over 1183 it fires blue-black with rust brown where it gathers. Recommended Cone 4-6
1431 Pearl White Floating Stoneware Glaze 1431P A warm pearl white with a soft grey bloom, lighter over raised texture. Recommended Cone 4-6
1432 Curry Floating Stoneware Glaze 1432P A mustard gold with an olive cast, paler over raised edges. Recommended Cone 4-6
1433 Twilight Floating Stoneware Glaze 1433P A near-black that floats steel grey over texture. Recommended Cone 4-6
1434 Autumn Purple Floating Stoneware Glaze 1434P A plum purple floating a dusty blue-lilac, with rust showing where thin. Recommended Cone 4-6
1435 Sangria Floating Stoneware Glaze 1435P A deep wine red with a darker mottle, breaking to rust at the edges. Recommended Cone 4-6