Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Spectrum  |  1405P

1405 Blue Oyster Shino Glaze

A soft blue-grey.

$24

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 1400 series is a cone 4/6 shino glaze. The surface is a satin matte at cone 5 and a little glossier at cone 6. It is made to break, so the colour deepens where the glaze sits thicker and the clay body shows through where it runs thinnest, and the effect is stronger at cone 6. Three brush coats give the full colour. Spectrum rates the series cone 4 to 6, 1190 to 1230°C. Lead-free and non-toxic.

  • Cone 4 to 6, 1190 to 1230°C
  • A soft blue-grey
  • Satin matte at cone 5, glossier at cone 6
  • Breaks where the thickness varies
  • Three brush coats
  • Lead-free and non-toxic