1140 Texture Kiwi Fruit Stoneware Glaze 1140P A bright green flecked with yellow and dark blue-green. Recommended Cone 4-6
1141 Texture Cascade Stoneware Glaze 1141P A muted mauve tan, faintly iridescent. Recommended Cone 4-6
1143 Texture Navy Stoneware Glaze 1143P A deep navy banded with lighter violet blue. Recommended Cone 4-6
1146 Texture Swampy Stoneware Glaze 1146P A dark blue-black streaked with olive and rust. Recommended Cone 4-6
1148 Texture Chowder Stoneware Glaze 1148P A pale cream yellow with a rust break. Recommended Cone 4-6
1156 Olive Stone Stoneware Glaze 1156P A dark olive brown, breaking yellow-green. Recommended Cone 4-6
1157 Texture Honey Stoneware Glaze 1157P A golden amber, ringed with paler spots. Recommended Cone 4-6
1158 Texture Bronze Stoneware Glaze 1158P An olive bronze, banded dark and gold. Recommended Cone 4-6
1161 Texture Topaz Stoneware Glaze 1161P A soft tan olive, breaking rust orange. Recommended Cone 4-6
1162 Texture Burgundy Stoneware Glaze 1162P A crimson magenta banded with orange. Recommended Cone 4-6