Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Spectrum  |  1146P

1146 Texture Swampy Stoneware Glaze

A dark blue-black streaked with olive and rust.

$24

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 1100 series is a cone 4/6 stoneware glaze, and this colour is reactive. It is made to move and change in the firing instead of laying down one flat colour, so the result depends on the temperature, how thickly it is applied and the clay underneath, and the same jar can look quite different on a different body. Three brush coats give the full colour. A reduction firing gives a different result from an electric kiln. Lead-free.

  • Cone 4 to 6, cone 5 recommended
  • A dark blue-black streaked with olive and rust
  • Reactive, varies with temperature, thickness and clay body
  • Three brush coats
  • Lead-free