Spectrum | 1139P
1139 Chrome Green Stoneware Glaze
A dark forest green opaque gloss.
$20
Suggested retail price. In-store prices and availability may vary by location.
Spectrum's 1100 series is a line of opaque gloss stoneware glazes made mainly from frits and stains, which gives strong, even colour. Apply three smooth brush coats to cone 04 bisque and fire to cone 5. Spectrum rates the series cone 4 to 6. It can also be dipped, thinned with a little water if needed. Lead free, ACMI AP non toxic and dinnerware safe. Fire a test tile with each new batch.
- Cone 5, rated cone 4 to 6
- Dark forest green, opaque gloss
- Three brush coats over cone 04 bisque
- Brush or dip
- Lead free, ACMI AP non toxic, dinnerware safe