Spectrum | 1401P
1401 Cherry Salmon Shino Glaze
A warm coral red.
$24
Suggested retail price. In-store prices and availability may vary by location.
Spectrum's 1400 series is a cone 4/6 shino glaze. The surface is a satin matte at cone 5 and a little glossier at cone 6. It is made to break, so the colour deepens where the glaze sits thicker and the clay body shows through where it runs thinnest, and the effect is stronger at cone 6. Three brush coats give the full colour. Spectrum rates the series cone 4 to 6, 1190 to 1230°C. Lead-free. Spectrum does not rate it non-toxic in the liquid state.
- Cone 4 to 6, 1190 to 1230°C
- A warm coral red
- Satin matte at cone 5, glossier at cone 6
- Breaks where the thickness varies
- Three brush coats
- Lead-free
- Not rated non-toxic in the liquid state