Spectrum | 1404P
1404 Wasabi Shino Glaze
A soft olive green.
$24
Suggested retail price. In-store prices and availability may vary by location.
Spectrum's 1400 series is a cone 4/6 shino glaze. The surface is a satin matte at cone 5 and a little glossier at cone 6. It is made to break, so the colour deepens where the glaze sits thicker and the clay body shows through where it runs thinnest, and the effect is stronger at cone 6. Three brush coats give the full colour. Spectrum rates the series cone 4 to 6, 1190 to 1230°C. Lead-free and non-toxic.
- Cone 4 to 6, 1190 to 1230°C
- A soft olive green
- Satin matte at cone 5, glossier at cone 6
- Breaks where the thickness varies
- Three brush coats
- Lead-free and non-toxic