1436 Kimchi Floating Stoneware Glaze 1436P A brick red-orange with a lighter rust float, paler over texture. Recommended Cone 4-6
1437 Floating Celadon Stoneware Glaze 1437P A soft sage green floating a paler grey-green over texture. Recommended Cone 4-6
1438 Cactus Floating Stoneware Glaze 1438P A leaf green with a yellow-green float, lighter over raised edges. Recommended Cone 4-6
1439 Nori Green Floating Stoneware Glaze 1439P A deep bottle green that floats a lighter olive over texture. Recommended Cone 4-6
1440 Floating Blue Stoneware Glaze 1440P A slate blue-black that floats a lighter grey-blue over texture. Recommended Cone 4-6
1441 Scandinavian Blue Floating Stoneware Glaze 1441P A deep glossy navy, paler over raised edges. Recommended Cone 4-6
1442 Glacier Floating Stoneware Glaze 1442P A pale grey-blue with a white float over texture. Recommended Cone 4-6
1443 Fuzzy Peach Floating Stoneware Glaze 1443P A warm peach tan floating a lighter apricot over texture. Recommended Cone 4-6
1444 Tiger Eye Floating Stoneware Glaze 1444P A caramel brown with a darker amber mottle, lighter over raised edges.
1445 Papaya Floating Stoneware Glaze 1445P A bright orange-red that floats a paler orange over texture. Recommended Cone 4-6
1446 Sunrise Floating Stoneware Glaze 1446P A soft coral orange with a pink float over texture. Recommended Cone 4-6
1447 Bougainvillea Floating Stoneware Glaze 1447P A raspberry red floating a paler pink over raised edges. Recommended Cone 4-6
1448 Shallot Floating Stoneware Glaze 1448P A dusty rose-purple with a plum mottle, lighter over texture. Recommended Cone 4-6
1449 Floating Turquoise Stoneware Glaze 1449P A muted teal that floats a pale turquoise over texture. Recommended Cone 4-6
1450 Morning Glory Floating Stoneware Glaze 1450P A pale periwinkle blue with a white float over raised edges. Recommended Cone 4-6
1451 Louisiana Bayou Floating Stoneware Glaze 1451P A near-black blue-green with a dark teal float over texture. Recommended Cone 4-6
1452 Spanish Moss Floating Stoneware Glaze 1452P A grey-green sage floating a pale silvery green over texture. Recommended Cone 4-6
1453 Ginger Floating Stoneware Glaze 1453P A warm ginger brown floating a pale rose-beige over texture. Recommended Cone 4-6
1454 Tapenade Floating Stoneware Glaze 1454P A dark olive-brown, close to black, with a lighter olive float over texture. Recommended Cone 4-6
1462 Rainy Day Semi-Transparent Glaze 1462P A muted grey with a green cast, deepening where the glaze gathers. Recommended Cone 4-6
1463 Cerulean Semi-Transparent Glaze 1463P A pale turquoise that reads clearly blue-green. Recommended Cone 4-6
1465 Light Celadon Semi-Transparent Glaze 1465P A very pale sage, barely tinted. Recommended Cone 4-6