Spectrum | 1465P
1465 Light Celadon Semi-Transparent Glaze
A very pale sage, barely tinted.
$14.50
Suggested retail price. In-store prices and availability may vary by location.
Spectrum's 1460 series is a cone 4/6 stoneware glaze with a semi-transparent high gloss surface. It darkens where it pools in carved and impressed detail and stays clear enough to show an underglaze design through it. Three brush coats on low-fired bisque give the full colour. Spectrum rates the series cone 4 to 6, 1190 to 1230°C. Lead-free and AP non-toxic. Conforms to ASTM D-4236.
- Cone 4 to 6, 1190 to 1230°C
- A very pale sage, barely tinted
- Semi-transparent high gloss, darkens where it pools
- Three brush coats
- Lead-free and AP non-toxic
- Conforms to ASTM D-4236