Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Spectrum  |  1436P

1436 Kimchi Floating Stoneware Glaze

A brick red-orange with a lighter rust float, paler over texture.

$26

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 1430 series is a cone 4/6 stoneware glaze made to look like one colour floating on another: a second colour rises to the surface in the firing, and the glaze breaks lighter over rims, edges, and texture. It is a glossy reactive glaze, so the result shifts with firing temperature (cone 6 fires differently from cone 5), glaze thickness, and the clay body; Spectrum has fired it on white, buff, red, and black bodies. Apply three brush coats to bisque and fire to cone 5. Spectrum rates the series cone 4 to 6, 1190 to 1230°C. Lead-free, ACMI AP non-toxic, and dinnerware safe.

  • Cone 5, rated cone 4 to 6, 1190 to 1230°C
  • A brick red-orange with a lighter rust float, paler over texture
  • Floating glaze: a second colour rises in the firing and breaks over texture
  • Reactive: varies with temperature, thickness, and clay body
  • Three brush coats
  • Lead-free, ACMI AP non-toxic, dinnerware safe