Spectrum | 1452P
1452 Spanish Moss Floating Stoneware Glaze
A grey-green sage floating a pale silvery green over texture.
$21
Suggested retail price. In-store prices and availability may vary by location.
Spectrum's 1430 series is a cone 4/6 stoneware glaze made to look like one colour floating on another: a second colour rises to the surface in the firing, and the glaze breaks lighter over rims, edges, and texture. It is a glossy reactive glaze, so the result shifts with firing temperature (cone 6 fires differently from cone 5), glaze thickness, and the clay body; Spectrum has fired it on white, buff, red, and black bodies. Apply three brush coats to bisque and fire to cone 5. Spectrum rates the series cone 4 to 6, 1190 to 1230°C. Lead-free, ACMI AP non-toxic, and dinnerware safe.
- Cone 5, rated cone 4 to 6, 1190 to 1230°C
- A grey-green sage floating a pale silvery green over texture
- Floating glaze: a second colour rises in the firing and breaks over texture
- Reactive: varies with temperature, thickness, and clay body
- Three brush coats
- Lead-free, ACMI AP non-toxic, dinnerware safe