Spectrum | 1187P
1187 Clear Crackle Stoneware Glaze
A clear glaze that fires to a fine crazed web.
$16
Suggested retail price. In-store prices and availability may vary by location.
This is one of Spectrum's 1100 series stoneware glazes. The surface is a clear crackle. The pattern forms as the piece cools and takes coloured dye. Brush on three coats for full colour and fire to cone 5, which is where it will match the jar. It will fire anywhere from cone 4 to cone 6, 1190 to 1230°C, but expect the result to shift a little at either end. It is not dinnerware safe, because the crazing can hold bacteria, so keep it off surfaces that touch food or drink. Lead-free and AP non-toxic. Conforms to ASTM D-4236.
- Cone 4 to 6, cone 5 recommended
- A clear glaze that fires to a fine crazed web
- Clear crackle
- Three brush coats
- Not dinnerware safe, the crazing can hold bacteria
- Lead-free and AP non-toxic
- Conforms to ASTM D-4236