Spectrum | 1112P
1112 Gold Stoneware Glaze
A warm bronze brown with a metallic sheen.
$20
Suggested retail price. In-store prices and availability may vary by location.
Spectrum's 1100 series is a cone 4/6 stoneware glaze, and this colour is reactive, tuned for a metallic result. It is made to move and change in the firing instead of laying down one flat colour, so the result depends on the temperature, how thickly it is applied and the clay underneath, and the same jar can look quite different on a different body. Three brush coats give the full colour. A reduction firing gives a different result from an electric kiln. Lead-free. Spectrum does not rate it non-toxic in the liquid state.
- Cone 4 to 6, cone 5 recommended
- A warm bronze brown with a metallic sheen
- Reactive metallic, varies with temperature, thickness and clay body
- Three brush coats
- Lead-free
- Not rated non-toxic in the liquid state