Spectrum | 1120P
1120 Satin Clear Stoneware Glaze
A satin clear with a faint yellow cast.
$16
Suggested retail price. In-store prices and availability may vary by location.
This is one of Spectrum's 1100 series stoneware glazes. The surface is a clear satin. It is less translucent than a clear gloss and mutes underglaze colour somewhat. Brush on three coats for full colour and fire to cone 5, which is where it will match the jar. It will fire anywhere from cone 4 to cone 6, 1190 to 1230°C, but expect the result to shift a little at either end. Lead-free and AP non-toxic. Conforms to ASTM D-4236.
- Cone 4 to 6, cone 5 recommended
- A satin clear with a faint yellow cast
- Clear satin
- Three brush coats
- Lead-free and AP non-toxic
- Conforms to ASTM D-4236