Spectrum | 1123P
1123 Satin Speckle Stoneware Glaze
An off-white with fine rust speckle.
$20
Suggested retail price. In-store prices and availability may vary by location.
This is one of Spectrum's 1100 series stoneware glazes. It fires to an opaque satin, so the clay body will not show through. Brush on three coats for full colour and fire to cone 5, which is where it will match the jar. It will fire anywhere from cone 4 to cone 6, 1190 to 1230°C, but expect the colour to shift a little at either end. Lead-free and AP non-toxic. Conforms to ASTM D-4236.
- Cone 4 to 6, cone 5 recommended
- An off-white with fine rust speckle
- Opaque satin
- Three brush coats
- Lead-free and AP non-toxic
- Conforms to ASTM D-4236