Spectrum | 1111P
1111 Holly Green Stoneware Glaze
A very dark green, breaking to pale green where it thins.
$20
Suggested retail price. In-store prices and availability may vary by location.
This is one of Spectrum's 1100 series stoneware glazes. The surface is a semi-transparent gloss, so the clay body reads through the colour. Brush on three coats for full colour and fire to cone 5, which is where it will match the jar. It will fire anywhere from cone 4 to cone 6, 1190 to 1230°C, but expect the result to shift a little at either end. Lead-free. Spectrum does not rate it non-toxic in the liquid state.
- Cone 4 to 6, cone 5 recommended
- A very dark green, breaking to pale green where it thins
- Semi-transparent gloss
- Three brush coats
- Lead-free
- Not rated non-toxic in the liquid state