Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Spectrum  |  1109P

1109 Coral Stoneware Glaze

A warm orange-pink.

$16

Suggested retail price. In-store prices and availability may vary by location.

This is one of Spectrum's 1100 series stoneware glazes. It fires to an opaque gloss, so the clay body will not show through. Brush on three coats for full colour and fire to cone 5, which is where it will match the jar. It will fire anywhere from cone 4 to cone 6, 1190 to 1230°C, but expect the colour to shift a little at either end. Lead-free and AP non-toxic. Conforms to ASTM D-4236.

  • Cone 4 to 6, cone 5 recommended
  • A warm orange-pink
  • Opaque gloss
  • Three brush coats
  • Lead-free and AP non-toxic
  • Conforms to ASTM D-4236