Snow Low Fire Clay
SNOW
Snow is a smooth, white-burning dolomite earthenware for low-fire work. Its fired shrinkage is effectively zero up to cone 4, so flat work stays flat – tiles come out of the kiln without warping or curling at the edges.
Recommended Cone 06-04