SiO-2 | PRAI3D
SiO-2 PRAI 3D Printing Stoneware
PRAI white stoneware made for 3D printing, at just the right moisture for the printer.
$42
Suggested retail price. In-store prices and availability may vary by location.
This is the same PRAI body, with 40 percent impalpable grog and an ivory fired colour, adjusted to the ideal moisture for clay 3D printing. It dries and fires well, and gives glazes and colouring oxides a bright base.
- 1240 to 1300°C (about cone 7 to 10)
- 40 percent impalpable grog, up to 0.2 mm
- Shrinkage about 8 percent drying, 7.0 percent firing at 1300°C
- Absorption 0.0 percent at 1300°C
- 5 kg (11 lb) or 1.6 kg (3.5 lb) bag