SiO-2 | 14210001
SiO-2 PCLI Stoneware Paper Clay
A stoneware paper clay with exceptional plasticity, for shapes that would crack in an ordinary clay.
$49
Suggested retail price. In-store prices and availability may vary by location.
Paper fibres through the body help stop cracks and warping, so PCLI suits difficult shapes and pieces that are hard to dry evenly. It carries impalpable grog up to 0.2 mm, models beautifully, and it's odourless.
- 1100 to 1260°C (about cone 03 to 9), bisque at 1050°C
- Paper fibre and impalpable grog, up to 0.2 mm
- Shrinkage 6.7 percent drying, 5.8 percent firing at 1200°C
- Absorption 5.6 percent at 1200°C
- 1.8 kg (4 lb) bag