SiO-2 | 8606
SiO-2 Lagoon Turquoise Porcelain
A porcelain that fires to a range of turquoise blues, with the colour all the way through the clay.
$45
Suggested retail price. In-store prices and availability may vary by location.
The colour runs through the whole body, so carved or unglazed areas stay turquoise. Lagoon is very plastic, which makes it a pleasure to throw and model. Its stable formula fires safely from 1200 to 1240°C in oxidation, and it's rated food safe for tableware.
- 1200 to 1240°C (about cone 5 to 7), oxidation
- No grog, smooth porcelain
- Shrinkage 5.6 percent drying, 10.6 percent firing at 1240°C
- Absorption 0.0 percent at 1240°C
- Food safe for tableware
- 5 kg (11 lb) or 1.6 kg (3.5 lb) bag