SiO-2 | 8504
SiO-2 Marte Red Sculpture Clay
A grogged red clay for sculpture and murals, with reds that deepen as the temperature climbs.
$44
Suggested retail price. In-store prices and availability may vary by location.
Marte carries 40 percent fine grog up to 0.5 mm, which gives it a textured surface and keeps it steady through drying and firing. It's made for sculpture and decorative murals, and its red tones grow richer the hotter you fire.
- 1100 to 1260°C (about cone 03 to 9)
- 40 percent fine grog, up to 0.5 mm
- Shrinkage 6.6 percent drying, 3.8 percent firing at 1260°C
- Absorption 8.6 percent at 1260°C
- 12.5 kg (27.6 lb) or 1.8 kg (4 lb) bag