567 Fire Engine Red Underglaze 567 A clean strong true red that holds its colour bare almost as well as it does under a clear glaze. Recommended Cone 06-6
569 Neon Orange Underglaze 569 An intense red-orange, closer to scarlet than to orange. Recommended Cone 06-6
700 Clear Gloss Glaze 700P A clear gloss that fires to a bright transparent film. Recommended Cone 06-04
701 Snow White Opaque Gloss Glaze 701 An opaque white with a faint cream warmth, not a stark blue-white. Recommended Cone 06-04
702 Porcelain White Opaque Gloss Glaze 702 A cool opaque white with a whisper of grey-green. Recommended Cone 06-04