Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Spectrum  |  701

701 Snow White Opaque Gloss Glaze

An opaque white with a faint cream warmth, not a stark blue-white.

$20

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 700 series is a low fire gloss glaze with solid, opaque colour, so the clay underneath does not show through. Two to three brush coats give full coverage. These colours do not tend to bleed, so one can be painted right up against another. Spectrum rates the series cone 06 to 04, 1015 to 1060°C. Lead-free and AP non-toxic. Conforms to ASTM D-4236.

  • Cone 06 to 04, 1015 to 1060°C
  • An opaque white with a faint cream warmth to it rather than a stark blue-white finish
  • Opaque coverage in 2 to 3 brush coats
  • Does not tend to bleed, so colours can usually be placed edge to edge
  • Lead-free and AP non-toxic, no cadmium
  • Conforms to ASTM D-4236