703 Light Gray Opaque Gloss Glaze 703P A pale soft grey with a faint green cast, opaque and glossy. Recommended Cone 06-04
706 Royal Blue Opaque Gloss Glaze 706P A deep saturated blue leaning slightly to violet, opaque and very glossy. Recommended Cone 06-04
707 Azure Opaque Gloss Glaze 707P A mid periwinkle with a clear violet cast, opaque and glossy. Recommended Cone 06-04
708 Baby Blue Opaque Gloss Glaze 708P A soft light aqua, blue with a definite green in it, opaque and glossy. Recommended Cone 06-04
709 Powder Blue Opaque Gloss Glaze 709P A soft mid blue with a slight grey-green cast, opaque and glossy. Recommended Cone 06-04
711 Navy Blue Opaque Gloss Glaze 711P A very dark blue that reads almost black until the light catches it, opaque and very glossy. Recommended Cone 06-04
713 Hunter Green Opaque Gloss Glaze 713P A deep pine green with a slight blue lean, opaque and very glossy. Recommended Cone 06-04
714 Sea Spray Opaque Gloss Glaze 714P A mid teal sitting evenly between blue and green, opaque and glossy. Recommended Cone 06-04
715 Mint Opaque Gloss Glaze 715P A soft pale green with a faint grey cast, opaque and glossy. Recommended Cone 06-04
716 Jade Opaque Gloss Glaze 716P A mid green with a clear blue lean, opaque and glossy. Recommended Cone 06-04
717 Forest Green Opaque Gloss Glaze 717P A very dark green that reads near-black across a flat surface. Recommended Cone 06-04
718 Mahogany Opaque Gloss Glaze 718P A very deep red-brown, near-black in the flat. Recommended Cone 06-04
721 Desert Sand Opaque Gloss Glaze 721P A warm mid tan about the tone of milky coffee, opaque and glossy. Recommended Cone 06-04
723 Chocolate Brown Opaque Gloss Glaze 723P A very dark brown, near-black in the flat. Recommended Cone 06-04
724 Mango Opaque Gloss Glaze 724P A strong warm orange sitting slightly to the yellow side, opaque and very glossy. Recommended Cone 06-04
726 Ivory Opaque Gloss Glaze 726P A soft warm off-white with a faint olive cast, opaque and glossy. Recommended Cone 06-04
727 Blush Opaque Gloss Glaze 727P A soft mid coral, warm and slightly earthy, closer to terracotta than to pink. Recommended Cone 06-04
730 Deep Pink Opaque Gloss Glaze 730P A strong cool pink leaning to crimson, opaque and very glossy. Recommended Cone 06-04
731 Rose Opaque Gloss Glaze 731P A soft dusty pink with a warm brown undertone, opaque and glossy. Recommended Cone 06-04
732 Powder Pink Opaque Gloss Glaze 732P A clear mid rose, cooler and cleaner than a dusty tone. Recommended Cone 06-04