761 Grass Green Opaque Gloss Glaze 761P A bright clear mid green with a yellow lean, opaque and very glossy. Recommended Cone 06-04
762 Dove Gray Opaque Gloss Glaze 762P A soft pale grey with a warm cast, opaque and glossy. Recommended Cone 06-04
763 Black Velvet Opaque Gloss Glaze 763P A dense true black under a very high gloss. Recommended Cone 06-04
802 Ivory Speckle Semi-Transparent Glaze 802P A soft cream, finely flecked with rust-brown speckle. Recommended Cone 06-04
805 Spiced Honey Semi-Transparent Glaze 805P A warm honey yellow under heavy rust-brown speckle. Recommended Cone 06-04
806 Brown Sugar Semi-Transparent Glaze 806P A light tan brown, streaked and lightly speckled. Recommended Cone 06-04
808 Clear Blue Semi-Transparent Glaze 808P A pale watery blue-grey, thinning almost clear where it doesn't pool. Recommended Cone 06-04
809 Clear Pink Semi-Transparent Glaze 809P A soft warm flesh tone rather than a cool pink. Recommended Cone 06-04
812 Beanpot Brown Semi-Transparent Glaze 812P A mid russet brown with darker speckle. Recommended Cone 06-04
813 Denim Blue Semi-Transparent Glaze 813P A deep saturated cobalt, darker still where it pools. Recommended Cone 06-04
822 Emerald Green Semi-Transparent Glaze 822P A deep green that lightens markedly where it thins. Recommended Cone 06-04
824 Grape Semi-Transparent Glaze 824P A dark aubergine, lighter where it thins. Recommended Cone 06-04
825 Umber Semi-Transparent Glaze 825P A rust orange-brown, strongly banded light to dark. Recommended Cone 06-04
850 Clear Raku Glaze 850P A clear glaze that fires to a fine dark crackle web over the body. Recommended Cone 08
852 Turquoise Raku Glaze 852P A bright turquoise, edged with dark copper flashing. Recommended Cone 08