521 Sand Underglaze 521 A warm khaki-buff with an olive cast - oatmeal rather than beach sand. Recommended Cone 06-6
530 Hunter Green Underglaze 530 A very dark green with a blue tinge, near-black under a clear glaze. Recommended Cone 06-6
534 Lavender Underglaze 534Z A mid periwinkle that reads more blue than lavender. Recommended Cone 06-6
537 Cobalt Blue Underglaze 537 A deep true cobalt under a clear glaze, settling to a softer faded mid blue where left bare. Recommended Cone 06-6
540 Denim Blue Underglaze 540 Indigo under a clear glaze, dropping to a pale chalky grey-blue where left bare - a wide difference between the two finishes. Recommended Cone 06-6
541 Purple Underglaze 541 A near-black aubergine, dark enough to read almost black. Recommended Cone 06-6