Self Supporting Pyrometric Cone 3
SSB3
Cone 3 in Orton's self supporting series. It stands on the shelf on its own moulded base, so there is no plaque to set and no mounting height to get wrong, and its bend after the firing shows whether the ware reached cone 3.