Our email is currently down – please call us if you are trying to get in touch.

Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Orton  |  SSB9

Self Supporting Pyrometric Cone 9

Cone 9 in Orton's self supporting series. It stands on the shelf on its own moulded base, so there is no plaque to set and no mounting height to get wrong, and its bend after the firing shows whether the ware reached cone 9.

$25

Suggested retail price. In-store prices and availability may vary by location.

This is Cone 9 in Orton's self supporting SSB series. Orton lists it bending at 1224°C (2235°F) at 15°C an hour, 1260°C (2300°F) at 60°C an hour and 1280°C (2336°F) at 150°C an hour, each measured over the last 100°C of the firing. A cone responds to time and temperature together, not temperature alone, so the rate the kiln is climbing at decides which of those numbers applies. The base is moulded into the cone, so it stands on the kiln shelf straight from the box with no plaque or wire holder, and the height and 8 degree lean are set at the factory. That makes it the usual choice for witness cones and test firings. Orton lists cones in this part of the range for porcelain, stoneware, china and floor tile. It has finished bending when the tip is level with the base.

  • Cone 9
  • Box of 25 cones
  • Bends 1224°C (2235°F) at 15°C an hour
  • Bends 1260°C (2300°F) at 60°C an hour
  • Bends 1280°C (2336°F) at 150°C an hour
  • 63.5 mm (2½ in) tall
  • Base moulded in, no plaque, clay pat or wire holder needed
  • Height and 8 degree lean set at the factory
  • Finished when the tip is level with the base

Downloads

Orton’s cone charts and guide to cones and firing.