CO-6 Supernova Cosmos Crystalline Glaze CO-6 Supernova is a highly fluid creamy white translucent glaze with a crystalline surface like frost on a window. The gloss glaze surface is opalescent and breaks slightly more cream than white. Recommended Cone 5-6
CO-7 Solar Flare Cosmos Crystalline Glaze CO-7 Solar Flare is a highly fluid light brown glaze with an iridescent crystalline surface. Opaque and glossy with a slight texture on the crystals. Recommended Cone 5-6
CO-8 Dark Star Cosmos Crystalline Glaze CO-8 Dark Star is a fluid, dark matte glaze with iridescent crystals like a beetle shell. Breaks translucent. Recommended Cone 5-6
Ceramic Decal – Blue Roses and Leaves DC100BL An underglaze transfer of blue roses and leaves, printed on rice paper for greenware or bisque.
Ceramic Decal – Black Roses and Leaves DC100BLK An underglaze transfer of black roses and leaves, printed on rice paper for greenware or bisque.
Ceramic Decal – Blue Butterflies DC20MB An underglaze transfer of blue butterflies, printed on rice paper for greenware or bisque.
Ceramic Decal – Flowers on Black DC33 An underglaze transfer of small pale flowers on a black ground, printed on rice paper for greenware or bisque.
Ceramic Decal – Flowers on Blue DC33MB An underglaze transfer of small pale flowers on a blue ground, printed on rice paper for greenware or bisque.
Ceramic Decal – Blue Ferns DC64MB An underglaze transfer of small blue fern leaf shapes in a geometric repeat, printed on rice paper for greenware or bisque.
Ceramic Decal – Blue Sea Life DC75MB An underglaze transfer of blue sea life, including fish, octopus, crabs, lobster and shells, printed on rice paper for greenware or bisque.
KI-11 Snow Drift Kiln Ice Crackle Glaze KI-11 Snow Drift is a diffused, milky white glaze. Recommended Cone 5-6
KI-18 Arctic Blush Kiln Ice Crackle Glaze KI-18 Arctic Blush is a pastel pink glaze, with a delicate, milky quality. Recommended Cone 5-6
KI-21 Winter Glass Kiln Ice Crackle Glaze KI-21 Winter Glass is a pastel, frosty blue. Recommended Cone 5-6
KI-27 Glacial Lake Kiln Ice Crackle Glaze KI-27 Glacial Lake is a vibrant blue-green hue. Recommended Cone 5-6
KI-46 Frozen Fern Kiln Ice Crackle Glaze KI-46 Frozen Fern is a muddled yellow-green hue. Recommended Cone 5-6
KI-68 Honey Crystal Kiln Ice Crackle Glaze KI-68 Honey Crystal is a warm, golden, and buttery yellow colour. Recommended Cone 5-6
Redwood Matte Moroccan Sand Glaze MS-12 Redwood Matte is a warm russet red-brown, mottled with faint rust flecking and lifting lighter on raised detail. Recommended Cone 5-6
Lemon Yellow Moroccan Sand Glaze MS-13 Lemon Yellow is a soft pale lemon, even, breaking to cream on raised detail. Recommended Cone 5-6
Ochre Moroccan Matte Glaze MS-15 Ochre is a warm golden mustard, mottling darker across the field and lifting to honey on raised detail. Recommended Cone 5-6
Robin’s Egg Moroccan Fusion Glaze MS-18 Robin's Egg is a soft duck-egg blue-green, breaking to pale cream over raised detail. Recommended Cone 5-6
Royal Blue Moroccan Fusion Glaze MS-20 Royal Blue is a strong saturated cobalt, even, lifting to a pale powder blue where thin. Recommended Cone 5-6
Dark Turquoise Moroccan Matte Glaze MS-23 Dark Turquoise is a dusty slate blue carrying fine darker speckle, with only a hint of teal in it. Recommended Cone 5-6
Peacock Moroccan Sand Glaze MS-27 Peacock is a soft pale grey-blue that pools to a deeper blue in recesses and breaks near-white on raised detail. Recommended Cone 5-6
Clear Bright Moroccan Sand Glaze MS-29 A glossy clear that fits many claybodies. Recommended Cone 5-6