C-33 Sandalwood Celadon Gloss Glaze C-33 A semi-translucent warm light brown like a sandy dune. Recommended Cone 5-6
C-36 Iron Celadon Gloss Glaze C-36 A glossy medium brown that pools darker brown and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-40 Aqua Celadon Gloss Glaze C-40 A light, glossy blue-green that pools darker turquoise and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-41 Pear Celadon Gloss Glaze C-41 A bright, glossy yellow-green that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-42 Saguaro Celadon Gloss Glaze C-42 A translucent pale soft green like a tall cactus. Recommended Cone 5-6
C-43 Wasabi Celadon Gloss Glaze C-43 A soft, glossy medium green that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-47 Jade Celadon Gloss Glaze C-47 A cool, glossy emerald green that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-49 Rainforest Celadon Gloss Glaze C-49 A deep, glossy forest green that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-5 Charcoal Celadon Gloss Glaze C-5 A deep translucent grey that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-50 Cherry Blossom Celadon Gloss Glaze C-50 A glossy, soft, blushing pink that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-52 Red Rock Celadon Gloss Glaze C-52 A semi-translucent deep russet brown like a Southwestern mesa. Recommended Cone 5-6
C-53 Weeping Plum Celadon Gloss Glaze C-53 A soft, glossy raspberry red that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-54 Snapdragon Celadon Gloss Glaze C-54 A bright, glossy red that accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-55 Poppy Celadon Gloss Glaze C-55 A light red that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-56 Lavender Celadon Gloss Glaze C-56 A cool, glossy lavender purple that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-57 Mulberry Celadon Gloss Glaze C-57 A deep, glossy purple that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-60 Marigold Celadon Gloss Glaze C-60 A glossy, deep yellow that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
C-65 Tangelo Celadon Gloss Glaze C-65 A transparent orange that pools and accents textured ware like the ancient glazes it is created to imitate. Recommended Cone 5-6
Choxil Underglaze Drawing Stick CHX A solid underglaze drawing stick for adding line and colour to bisque ware. Recommended Cone 04-6
CO-13 Mars Crystal Cosmos Crystalline Glaze CO-13 Mars Crystal is a highly fluid, dark brick red glaze with silvery, iridescent crystals that breaks darker over edges. Recommended Cone 5-6
CO-14 Solar Rainbow Cosmos Crystalline Glaze CO-14 Solar Rainbow is a highly fluid, dark gloss glaze with iridescent rainbow crystals. Breaks translucent. Recommended Cone 5-6
CO-24 Blue Starlight Cosmos Crystalline Glaze CO-24 Blue Starlight is a royal blue crystalline glaze with iridescent spiky crystals. It's a very deep colour, like looking into the night sky. Recommended Cone 5-6
CO-3 Event Horizon Cosmos Crystalline Glaze CO-3 Event Horizon is a dark, fluid glaze shifting between large crystals with blue and violet highlights at cone 5 and a bright gold surface at cone 6. Recommended Cone 5-6
CO-5 Dark Matter Cosmos Crystalline Glaze CO-5 Dark Matter is a deep, fluid glaze with shifting violet undertones and large rainbow crystals at cone 6. Crystals are smaller and more condensed at cone 5. Recommended Cone 5-6