H555 High Fire Clay

$49.32 / 20 kg (44 lb) Pugged

Suggested retail price. In-store prices and availability may vary by location.

High fired, Light grey-buff burning, Smooth, Medium plastic, Vitreous, Functional, Throwing clay body, Light specking in reduction

Specifications

Every figure is a measured range from the Plainsman lab, not a single nominal number. Cone equivalents are Orton self-supporting cones at 108 °F/hr.

Close-up of smooth, curved, beige ridges creating a flowing, wave-like pattern on a textured surface.

Description

H555 is a high-fire stoneware body designed for functional ware and made from a blend of refined and clean native clays. It fires vitreous – about 1% porosity at cone 10 – and performs well in both reduction and oxidation.

It is a pleasant throwing body: smooth and fine without feeling slick, and with high green strength. Its drying shrinkage is low for a high-fire body, so it dries with less cracking than most comparable bodies.

The firing atmosphere determines the colour. In reduction, H555 fires to a light grey-buff; in oxidation, it fires to a buff-white.