Low fired, Buff burning, Medium plastic, General purpose, Throwing and Hand-building clay body

Specifications

Every figure is a measured range from the Plainsman lab, not a single nominal number. Cone equivalents are Orton self-supporting cones at 108 °F/hr.

Close-up of beige corrugated cardboard with diagonal ribbed texture and shadow details.

Description

Full description for Buffstone coming soon.

You may also be Interested in

L210 Low Fire Clay

L210 is a smooth, silty, medium plastic earthenware for low-fire work. Its light raw colour makes it easy to clean up after, which is why it is a common choice for schools and teaching studios. It fires to a light warm orange red.

Recommended Cone 06-04

L212 Low Fire Clay

L212 is a smooth, medium plastic talc earthenware for low-fire work, firing to a light cream at cone 06 to 04. It is made for commercial low-fire glazes and is widely used in schools.

Recommended Cone 06-04

L215 Low Fire Clay

L215 is a smooth, plastic, red-burning terra cotta for low-fire work. It is built from a mix of our native red clays and our native stoneware, and it is good for throwing and hand-building.