Large Regular Pyrometric Cone 09
LRB09
Cone 09 in Orton's large regular series, the witness cone that stands on the kiln shelf beside the ware. Its bend after the firing shows whether the kiln reached, missed or passed cone 09, which a controller reading on its own cannot tell you.