Our email is currently down – please call us if you are trying to get in touch.

Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Plainsman Clays  |  WHEAT

Wheat Mid Fire Clay

$31.35 / 20 kg (44 lb) Pugged

Suggested retail price. In-store prices and availability may vary by location.

Mid fired, Warm buff burning, Light speck, Smooth, High plasticity, Throwing clay body

Description

Wheat is a smooth, highly plastic general purpose body for cone 6, firing to a warm buff. Iron concretions in the clay give it a light natural speck.

It is our lower-cost alternative to the M340 bodies. At cone 6 the maturity and colour are close to M340.

It is highly bentonitic, which is what gives it the plasticity – and means it needs less water than most throwing clays.

Specifications

Every figure is a measured range from the Plainsman lab, not a single nominal number. Cone equivalents are Orton self-supporting cones at 108 °F/hr.

Close-up of smooth beige plaster texture on a wall with subtle brush strokes and fine cracks.

You may also be Interested in