Our email is currently down – please call us if you are trying to get in touch.

Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Plainsman Clays  |  M340S

M340S Mid Fire Clay

$37.92 / 20 kg (44 lb) Pugged

Suggested retail price. In-store prices and availability may vary by location.

Mid fired, Light beige, Dark speckles, Medium to high plasticity, Silty, Throwing clay body

Specifications

Every figure is a measured range from the Plainsman lab, not a single nominal number. Cone equivalents are Orton self-supporting cones at 108 °F/hr.

Close-up image of evenly spaced, horizontal brown textured ridges creating a wave-like pattern.

Description

The speckle is deliberate: 0.3% granular manganese goes into the recipe. Do not judge the colour from the bag – in its pugged state M340S is a dark grey, and the light beige only arrives out of the kiln.

The clays that make it up are all mined locally in Saskatchewan, so the body has not travelled far to reach the plant and its environmental footprint is smaller than clays that must travel.

You may also be Interested in