Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Plainsman Clays  |  M340GS

M340GS Mid Fire Clay

$37.95 / 20 kg (44 lb) Pugged

Suggested retail price. In-store prices and availability may vary by location.

Mid fired, Light beige, Dark speckles, Grogged, Textured, Throwing and Hand-building clay body

Specifications

Every figure is a measured range from the Plainsman lab, not a single nominal number. Cone equivalents are Orton self-supporting cones at 108 °F/hr.

Close-up of smooth, curved, wave-like brown ridges creating an abstract, textured pattern.

Description

M340GS is a versatile medium-temperature clay body that combines the trusted performance of M340S with added fine grog. The grog opens the body, improves handling, and provides added structural support, making it an excellent choice for functional pottery, hand-building, and medium to larger forms. Granular manganese creates a warm, natural speckle that adds depth and character to glazed and unglazed surfaces.

In its pugged state, M340GS appears dark grey, but it transforms in the kiln to a soft, light beige. Some of the grog remains visible at the surface, giving finished pieces an appealing texture without overwhelming finer details. Its balanced feel and dependable strength make it a rewarding clay for potters who want both character and confidence in their work.

Made with clays mined locally in Canada, M340GS is a distinctive regional clay body with a shorter journey to our plant than imported materials. For makers seeking a strong, versatile medium-temperature body with natural texture, beautiful speckling, and a warm fired colour, M340GS is an outstanding choice.

You may also be Interested in