Our email is currently down – please call us if you are trying to get in touch.

Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Plainsman Clays  |  M350

M350 Mid Fire Clay

$40.99 / 20 kg (44 lb) Pugged

Suggested retail price. In-store prices and availability may vary by location.

Mid fired, Light red brown burning, Fine and smooth, Excellent green strength, Throwing clay body

Specifications

Every figure is a measured range from the Plainsman lab, not a single nominal number. Cone equivalents are Orton self-supporting cones at 108 °F/hr.

Close-up of textured brown fabric with wavy, folded patterns creating a 3D effect.

Description

M350 contains four different clays, each of them quite balanced on its own, all mined locally. That blend is why we have so much consistency and control over this body. It is similar in composition to M390, and shares the same very fine, smooth natural character.

The iron that occurs naturally in the clay reacts well with a lot of glaze recipes and gives a deeper colour response. Worth knowing before you plan a surface: the colour darkens considerably under a transparent glaze.

You may also be Interested in