Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Plainsman Clays  |  POLARICE

Polar Ice Mid Fire Porcelain

Suggested retail price. In-store prices and availability may vary by location.

Mid fired, Super white, Translucent, High plasticity, Vitreous, Porcelain, Throwing clay body

Specifications

Every figure is a measured range from the Plainsman lab, not a single nominal number. Cone equivalents are Orton self-supporting cones at 108 °F/hr.

Abstract close-up of smooth, curved white ridges creating a flowing, wave-like pattern.

Description

Full description for Polar Ice coming soon.

You may also be Interested in

P300 Mid Fire Porcelain

P300 is a smooth, off-white porcelain for cone 6 work. It fires whiter than M370 and close to Polar Ice, with plasticity that many potters rate at or above M370 – and it is not translucent at cone 6.

Recommended Cone 6

TOP SELLER M370 Mid Fire Clay

M370 Mid Fire Clay

M370 is one of our most popular white, medium-fired stoneware clay bodies. It has excellent plasticity, which makes it a pleasure to throw, and its lighter off-white colour gives you an ideal canvas for decorating.

Recommended Cone 6

TOP SELLER M340 Mid Fire Clay

M340 Mid Fire Clay

M340 is one of our most popular general-purpose clay bodies – plastic, medium-fired and buff burning, and it throws and hand-builds equally well. Best fired to cone 6.