Mid fired, White burning, Fine grained, Highly plastic, Throwing clay body

Specifications

Every figure is a measured range from the Plainsman lab, not a single nominal number. Cone equivalents are Orton self-supporting cones at 108 °F/hr.

Close-up of a beige surface with flowing, wavy textured lines creating a modern, abstract pattern.

Description

M370 is white because of what goes into it – more kaolins and fewer ball clays than our other bodies. That is what gives you the lighter off-white ground to decorate on, and it is why the powder makes a good base for slips and engobes.

M370 is mature at cone 6, but it is not fully vitreous – it remains partially vitrified, with absorption still measuring slightly above 0%. It has excellent plasticity, which allows for adding movement and alterations without complaints once a piece is thrown.

M370 is also available in dry form and as a casting recipe. The casting recipe contains no added bentonite, which allows for better drying within plaster moulds.