Our email is currently down – please call us if you are trying to get in touch.

Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Orton  |  SSB11

Self Supporting Pyrometric Cone 11

Cone 11 in Orton's self supporting series. It stands on the shelf on its own moulded base, so there is no plaque to set and no mounting height to get wrong, and its bend after the firing shows whether the ware reached cone 11.

$25

Suggested retail price. In-store prices and availability may vary by location.

This is Cone 11 in Orton's self supporting SSB series. Orton lists it bending at 1272°C (2322°F) at 15°C an hour, 1294°C (2361°F) at 60°C an hour and 1315°C (2399°F) at 150°C an hour, each measured over the last 100°C of the firing. A cone responds to time and temperature together, not temperature alone, so the rate the kiln is climbing at decides which of those numbers applies. The base is moulded into the cone, so it stands on the kiln shelf straight from the box with no plaque or wire holder, and the height and 8 degree lean are set at the factory. That makes it the usual choice for witness cones and test firings. Orton lists cones in this part of the range for porcelain, stoneware, china and floor tile. It has finished bending when the tip is level with the base.

  • Cone 11
  • Box of 25 cones
  • Bends 1272°C (2322°F) at 15°C an hour
  • Bends 1294°C (2361°F) at 60°C an hour
  • Bends 1315°C (2399°F) at 150°C an hour
  • 63.5 mm (2½ in) tall
  • Base moulded in, no plaque, clay pat or wire holder needed
  • Height and 8 degree lean set at the factory
  • Finished when the tip is level with the base

Downloads

Orton’s cone charts and guide to cones and firing.