This is Cone 022 in Orton's self supporting SSB series. Orton lists it bending at 586°C (1087°F) at 60°C an hour and 590°C (1094°F) at 150°C an hour, measured over the last 100°C of the firing. There is no 15°C an hour figure at this number, so only those two rates apply. A cone responds to time and temperature together, not temperature alone, so the rate the kiln is climbing at decides which of those numbers applies. The base is moulded into the cone, so it stands on the kiln shelf straight from the box with no plaque or wire holder, and the height and 8 degree lean are set at the factory. That makes it the usual choice for witness cones and test firings. Orton lists cones in this part of the range for overglaze decoration, lustres, enamels and decals, and for fusing, slumping and decorating glass. It has finished bending when the tip is level with the base.
- Cone 022
- Box of 25 cones
- Bends 586°C (1087°F) at 60°C an hour
- Bends 590°C (1094°F) at 150°C an hour
- No 15°C an hour figure published at this number
- 63.5 mm (2½ in) tall
- Base moulded in, no plaque, clay pat or wire holder needed
- Height and 8 degree lean set at the factory
- Finished when the tip is level with the base