Orton | SRB6
Small Pyrometric Cone 6 for Kiln-Sitter
Cone 6 in Orton's small series, made for the Dawson Kiln-Sitter. The sitter's sensing rod rests on it and the kiln shuts off as it bends, so this cone ends the firing instead of reporting on it afterwards.
$25
Suggested retail price. In-store prices and availability may vary by location.
This is Cone 6 in Orton's small regular SRB series, made for the Dawson Kiln-Sitter rather than the kiln shelf. Orton lists it bending at 1255°C (2291°F) at 300°C an hour, the only rate published for this size, measured in a gas fired kiln. The cone is tapered, so where the sensing rod sits on it makes a difference. The thin end fires cooler and the thick end hotter, and the gap between them is about half a cone. Small cones also bend 7 to 10°C (12 to 18°F) earlier than a self supporting cone of the same number, so do not use a self supporting figure for one of these. Orton lists cones in this part of the range for porcelain, stoneware, china and floor tile. If a firing comes out short, Orton says to load the next cone hotter into the Kiln-Sitter and put a witness cone on the shelf to see what the kiln actually reached.
- Cone 6
- Box of 50 cones
- Bends 1255°C (2291°F) at 300°C an hour, measured in a gas fired kiln
- 28.6 mm (1⅛ in) tall
- Sized for the Dawson Kiln-Sitter shut off
- Tapered, so its position under the sensing rod changes the result by about half a cone
- Bends 7 to 10°C (12 to 18°F) earlier than a self supporting cone
- Chart values assume a 23.8 mm (15/16 in) mounting height
Downloads
Orton’s cone charts and guide to cones and firing.