Our email is currently down – please call us if you are trying to get in touch.

Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Orton  |  SRB11

Small Pyrometric Cone 11 for Kiln-Sitter

Cone 11 in Orton's small series, made for the Dawson Kiln-Sitter. The sitter's sensing rod rests on it and the kiln shuts off as it bends, so this cone ends the firing instead of reporting on it afterwards.

$25

Suggested retail price. In-store prices and availability may vary by location.

This is Cone 11 in Orton's small regular SRB series, made for the Dawson Kiln-Sitter rather than the kiln shelf. Orton lists it bending at 1336°C (2437°F) at 300°C an hour, the only rate published for this size, measured in a gas fired kiln. The cone is tapered, so where the sensing rod sits on it makes a difference. The thin end fires cooler and the thick end hotter, and the gap between them is about half a cone. Small cones also bend 7 to 10°C (12 to 18°F) earlier than a self supporting cone of the same number, so do not use a self supporting figure for one of these. Orton lists cones in this part of the range for porcelain, stoneware, china and floor tile. If a firing comes out short, Orton says to load the next cone hotter into the Kiln-Sitter and put a witness cone on the shelf to see what the kiln actually reached.

  • Cone 11
  • Box of 50 cones
  • Bends 1336°C (2437°F) at 300°C an hour, measured in a gas fired kiln
  • 28.6 mm (1⅛ in) tall
  • Sized for the Dawson Kiln-Sitter shut off
  • Tapered, so its position under the sensing rod changes the result by about half a cone
  • Bends 7 to 10°C (12 to 18°F) earlier than a self supporting cone
  • Chart values assume a 23.8 mm (15/16 in) mounting height