Our email is currently down – please call us if you are trying to get in touch.

Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Orton  |  SRB014

Small Pyrometric Cone 014 for Kiln-Sitter

Cone 014 in Orton's small series, made for the Dawson Kiln-Sitter. The sitter's sensing rod rests on it and the kiln shuts off as it bends, so this cone ends the firing instead of reporting on it afterwards.

$25

Suggested retail price. In-store prices and availability may vary by location.

This is Cone 014 in Orton's small regular SRB series, made for the Dawson Kiln-Sitter rather than the kiln shelf. Orton lists it bending at 870°C (1598°F) at 300°C an hour, the only rate published for this size, measured in a gas fired kiln. The cone is tapered, so where the sensing rod sits on it makes a difference. The thin end fires cooler and the thick end hotter, and the gap between them is about half a cone. Small cones also bend 7 to 10°C (12 to 18°F) earlier than a self supporting cone of the same number, so do not use a self supporting figure for one of these. Orton lists cones in this part of the range for overglaze decoration, lustres, enamels and decals, and for fusing, slumping and decorating glass. If a firing comes out short, Orton says to load the next cone hotter into the Kiln-Sitter and put a witness cone on the shelf to see what the kiln actually reached.

  • Cone 014
  • Box of 50 cones
  • Bends 870°C (1598°F) at 300°C an hour, measured in a gas fired kiln
  • 28.6 mm (1⅛ in) tall
  • Sized for the Dawson Kiln-Sitter shut off
  • Tapered, so its position under the sensing rod changes the result by about half a cone
  • Bends 7 to 10°C (12 to 18°F) earlier than a self supporting cone
  • Chart values assume a 23.8 mm (15/16 in) mounting height

Downloads

Orton’s cone charts and guide to cones and firing.