Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Plainsman Clays  |  POLARICE-CAST

Polar Ice Casting Slip

Our whitest, most translucent cone 6 porcelain, made as a casting body and sold dry for mixing your own slip for plaster moulds.

$185 / 20 kg (44 lb)

$185

Suggested retail price. In-store prices and availability may vary by location.

Polar Ice Casting brings the brilliant white fired colour and translucency of Polar Ice porcelain to slip cast ware, and thin cast walls let light through. To make slip, mix the powder with water and Darvan No. 7, a deflocculant that keeps the slip fluid without extra water. Add most of the Darvan to the water first. Then add the powder slowly into the moving water with a propeller mixer so it disperses evenly. Keep back a little of the Darvan to adjust the flow at the end. Check the specific gravity after mixing and again the next day once the slip has settled. Specific gravity compares the weight of the slip with the same volume of water.

  • Cone 6, 1222°C (2232°F)
  • Brilliant white and translucent when fired
  • Sold dry in 20 kg (44 lb) and 2.5 kg (5.5 lb) bags
  • Mix with water and Darvan No. 7